Measuring the Bore and Choosing Oversize Rings

Piston rings are supplied in standard size and in oversizes to match a rebored cylinder. Ordering the wrong size wastes the set, and ordering standard rings for a worn bore wastes the whole rebuild. This article explains what to measure and how to choose the size.

Piston ring ကို standard နှင့် oversize အရွယ်အစားများဖြင့် ရရှိနိုင်သည်။ အရွယ်မှားပါက ring အစုံလုံး အလဟဿ ဖြစ်သည်။

Side view of a bore measured at top, middle and bottom, and a top view measured on two axes ninety degrees apart, defining taper and ovality.

Figure 1 — Where to measure a bore, and how taper and ovality are worked out. ပုံ 1 — Bore ကို မည်သည့်နေရာတွင် တိုင်းရမည်။

Standard and oversize

Ring sets are normally offered as STD (standard) and in oversizes such as 0.25 mm, 0.50 mm, 0.75 mm and 1.00 mm. The oversize refers to how much the cylinder has been bored out. Rings must match the finished bore, so the machining decision comes first and the ring order second.

Bore the cylinder first, then order the rings

Do not order rings before the machine shop has finished. The final bore size is decided by how much damage has to be removed, and it may come out larger than expected. Order to the measured finished bore, not to the intended one.

စက်ရုံမှ ပြီးဆုံးပြီးမှသာ ring မှာယူပါ။ အပြီးသတ် အရွယ်အစားသည် မျှော်မှန်းထားသည်ထက် ကြီးနိုင်သည်။

Measuring the bore

Use a bore gauge, not a vernier caliper. Measure each cylinder in at least three positions down its length and in two directions at right angles, then look for:

  • Taper — the bore worn wider at the top than the bottom, because the top of the stroke sees the highest pressure and the least lubrication.
  • Out-of-round — the bore worn oval rather than circular.
  • Scoring — vertical scratches from debris or seizure.

Compare against the manufacturer's wear limits for that engine. If taper or out-of-round exceeds the limit, new rings alone will not seal — the block must be bored and oversize pistons and rings fitted.

Honing and the crosshatch

A bore that is within limits still needs honing before new rings are fitted. Honing cuts a crosshatch pattern that holds oil and lets the new rings bed in. Fitting new rings into a glazed bore is one of the most common reasons a rebuild still burns oil afterwards.

Ring အသစ်မတပ်မီ bore ကို hone ရမည်။ Hone မလုပ်ဘဲ တပ်ပါက ဆီ ဆက်လောင်နေမည်။

What to tell us when ordering

  1. Vehicle make, model and year
  2. Engine code — essential, because one model often used several engines
  3. Number of cylinders
  4. The size required: STD or the oversize, taken from the finished bore measurement

ORDER & ENQUIRIES
မှာယူရန် နှင့် စုံစမ်းရန်

Phone  09 5105768  |  Email  support@winautoparts.com

Online  winautoparts.com  |  support.winautoparts.com (support portal and web chat)

South Dagon Distribution Centre  (172/173/174) Mawlamyine Street, Industrial Zone 1, South Dagon Township, Yangon — Mon–Sat 8:30 AM – 5:30 PM

Thakaytha Distribution Centre  Thakaytha Industrial Zone, Yangon — Mon–Sat 9:00 AM – 6:00 PM

Related Articles

 

Was this article helpful?
0 out of 0 found this helpful

Comments

0 comments

Please sign in to leave a comment.